- Overview
- Related Products
Materials are: low temperature 0Cr25Al5(below 900 degrees), medium temperature 0Cr21Al6Nb(below 1100 degrees), high temperature 0Cr27Al7Mo2(below 1200 degrees), ultra-high temperature material GH4136(below 1350 degrees), HYZ (1400 degrees) All temperatures refer to the air temperature in the furnace. Used in various types of electric heating heat treatment furnace. Our products have stable resistivity, high oxidation performance and improved surface power tolerance.
Product size: thickness 0.8-4mm, width: 6-150mm.
It can be processed into waves or other special shapes according to user needs.